Part 2 of a series on the engineering of electric vehicles
Just as a conventional combustion vehicle has a fuel tank that stores the fuel which powers its engine, an electric vehicle has a traction battery pack that stores the energy which powers its motor. The pack is the means by which energy is held on board and delivered to the vehicle on demand. The analogy, however, holds only up to a point. A fuel tank is a passive container: the chemical energy it holds is converted into work elsewhere, in the engine. A battery pack is an active electrochemical device. It both stores energy and converts it directly into electricity, it can be refilled while the vehicle is moving through regenerative braking, and it must be continuously monitored, cooled and protected. It is the heaviest and most expensive single component in the vehicle, and its design shapes almost every other engineering decision.
From Fuel Tank to Battery Pack
The contrast is clearest in numbers. A typical 50-litre petrol tank holds about 37 kg of fuel. At roughly 9.5 kWh per litre (34 MJ/L), that is close to 475 kWh of chemical energy, stored in a system weighing perhaps 50 kg when full [1]. A 75 kWh battery pack, by comparison, weighs in the region of 450–500 kg. Even after crediting the electric drivetrain with its three- to four-fold conversion-efficiency advantage (discussed in Part 1), the pack typically delivers only half to two-thirds of the range of that tank of fuel, at around ten times the mass.
Two further differences matter to the vehicle engineer. First, a fuel tank becomes lighter as it empties; a battery does not, so the vehicle carries its full energy-storage mass for the whole journey. Second, refuelling is extraordinarily fast. A pump delivering 40 litres per minute transfers chemical energy at an equivalent rate of more than 20 MW, whereas today’s fastest public chargers supply a few hundred kilowatts. Narrowing that gap without damaging the cells is one of the central problems of battery engineering.
The pack must also do something a fuel tank never does: it is the vehicle’s power source. It has to deliver several hundred kilowatts during hard acceleration and absorb high currents during regenerative braking. Battery engineers express current relative to capacity as the C-rate: a 1C discharge empties the battery in one hour, and a 2C discharge in thirty minutes. Cells are designed along a trade-off between specific energy and specific power. Thick electrodes store more energy, while thin electrodes allow lithium ions to move in and out faster and therefore deliver more power.
Inside the Cell: The Electrochemistry
The basic building block of the pack is the lithium-ion cell (Figure 1). Each cell has two electrodes, separated by a porous polymer film called the separator and soaked in a liquid electrolyte, typically the lithium salt LiPF6 dissolved in organic carbonate solvents [2], [3]. The negative electrode (the anode during discharge) is usually graphite coated on copper foil. The positive electrode (the cathode) is a lithium-containing metal oxide or phosphate coated on aluminum foil.
Figure 1. Operation of a lithium-ion cell during discharge. Lithium ions migrate through the electrolyte from the graphite anode to the cathode, while electrons travel through the external circuit and do work in the motor.
Both electrodes are intercalation hosts: their crystal structures can take lithium ions into the spaces between atomic layers and release them again without being destroyed. During discharge, lithium ions leave the graphite, cross the electrolyte, and enter the cathode, while the electrons they leave behind travel through the external circuit and drive the motor. During charging, the process reverses. Because lithium shuttles back and forth between two hosts, the design is often called a “rocking-chair” battery.
The cell voltage reflects the difference in the chemical potential of lithium in the two electrodes, related to the Gibbs free energy of the reaction by ΔG = −nFE. A cell with a nickel-rich cathode has a nominal voltage of about 3.6–3.7 V. A lithium iron phosphate (LFP) cell sits at about 3.2 V, and its discharge curve is unusually flat, which, as we will see in the next article, makes its state of charge difficult to estimate. On the first charge, a thin passivating layer called the solid electrolyte interphase (SEI) forms on the graphite surface. The SEI is essential, because it stops the electrolyte from decomposing further, but it permanently consumes some lithium, and its slow growth is a principal cause of ageing.
Choosing a Chemistry
The choice of cathode largely determines a cell’s energy density, cost, life and safety. The table summarises the main options. Figures are indicative ranges at cell level and vary considerably with design [3], [4].
| Chemistry | Specific energy (Wh/kg) | Cycle life | Thermal stability | Key characteristics |
|---|---|---|---|---|
| NMC (nickel manganese cobalt oxide) | 240–300 | 1,000–2,000 | Moderate | High energy; nickel-rich grades reduce cobalt content |
| NCA (nickel cobalt aluminium oxide) | 240–300 | 1,000–1,500 | Moderate | High energy; widely used in cylindrical cells |
| LFP (lithium iron phosphate) | 160–205 | 3,000+ | High | Low cost; free of nickel and cobalt; long life |
| Sodium-ion | 140–175 | Several thousand (claimed) | High | No lithium; good low-temperature performance; early commercial stage |
For most of the past decade, nickel-rich layered oxides dominated because range was the overriding priority. The balance has since shifted decisively. Helped by cell-to-pack designs that recover much of its density deficit at pack level, LFP accounted for nearly half of the global EV battery market in 2024 [5].
The anode is evolving too. Graphite stores at most 372 mAh/g, whereas silicon can theoretically store about 3,580 mAh/g. Silicon, however, swells by roughly 300% when fully lithiated. The resulting cyclic strain cracks particles and repeatedly ruptures the SEI, so commercial cells blend only modest fractions of silicon into graphite [6]. This is a recurring theme: many of the limits of battery chemistry turn out to be problems of mechanics. Solid-state batteries, which replace the liquid electrolyte with a ceramic or polymer solid and potentially allow a lithium-metal anode, face similar challenges. They must keep intimate contact at solid–solid interfaces under controlled stack pressure while suppressing lithium dendrites. Several manufacturers are in pilot production, but large-scale automotive deployment remains ahead of us.
Cell Formats
Cells are manufactured in three basic formats (Figure 2), each with distinct mechanical implications.
Figure 2. Cylindrical, prismatic and pouch cell formats.
Cylindrical cells wind long electrode strips into a “jelly roll” inside a steel can. The geometry is an efficient pressure vessel, and its hoop stiffness contains internal pressure and electrode swelling. Production is highly automated, and formats have grown from the 18650 to the 21700 and, more recently, the 46 mm-diameter 4680 cell, whose “tabless” current collection shortens the electrical path and eases heat removal [7]. Circles do not tile a plane, however: even in an ideal hexagonal arrangement, cylinders fill only about 91% (Ï€/2√3) of the available area. A pack can also contain thousands of cells, each needing welded connections.
Prismatic cells place wound or stacked electrodes in a rigid aluminium can. Their large capacity per cell means fewer interconnections and better space utilisation. The trade-off is that cell swelling over life must be resisted by end plates, straps or the pack structure itself, which must carry sustained compressive loads.
Pouch cells enclose stacked electrodes in a heat-sealed aluminium–polymer laminate. They are light and dimensionally flexible, but they have no structural strength of their own. The module must support them and apply a controlled compressive pressure, typically using compliant foam pads, to maintain electrode contact and accommodate swelling.
Pack Architecture
Cells are connected in series to build voltage and in parallel to build capacity, a configuration described as nSmP. Around 96 nickel-rich cells in series give a nominal voltage of roughly 350 V, the familiar “400 V-class” pack, and about twice that number gives an 800 V-class system. The attraction of higher voltage follows directly from P = VI: delivering 350 kW requires about 440 A at 800 V, against roughly 875 A at 400 V. Halving the current cuts resistive (I²R) losses in a given conductor by a factor of four, allowing lighter cables and faster charging, at the cost of components rated for the higher voltage.
Figure 3. A conventional module-based pack compared with a cell-to-pack design (schematic).
Traditionally, cells were grouped into modules, each with its own frame, end plates and wiring, and the modules were then installed in the pack enclosure. This hierarchy simplifies assembly and servicing, but the module structures take up space and add mass. Cell-to-pack (CTP) designs, introduced at scale around 2019–2020, remove the module layer altogether (Figure 3). BYD’s Blade battery, for example, uses long, thin LFP prismatic cells that themselves act as structural members, and the company reported a space-utilisation improvement of over 50% compared with conventional packs [8]. The next step, cell-to-body or cell-to-chassis integration, makes the pack part of the vehicle structure, with the pack lid serving as the cabin floor. The gains in packaging and stiffness come at a cost in repairability and ease of disassembly for recycling, since bonded structures cannot easily be taken apart.
The Pack as a Mechanical Structure
Here the mechanical engineer takes centre stage. The pack enclosure, usually aluminium extrusions and castings or high-strength steel, must protect the cells from underbody impacts with road debris and kerbs, and from intrusion during side-pole crashes, where the pack lies directly in the load path between the sills. It must survive years of road-induced vibration and shock, stay sealed against water and dust (typically to IP67), and vent safely if a cell fails. Inside, thermal interface materials and gap fillers conduct heat from the cells to liquid-cooled plates while also transmitting mechanical load. Swelling must be managed throughout the pack’s life, so that cells remain within their optimal pressure window as they age. When the pack is integrated into the body structure, it contributes to torsional stiffness, and its low, central mass lowers the vehicle’s centre of gravity. The pack is therefore a structural, thermal and electrochemical system all at once.
Safety and Degradation
The most serious failure mode is thermal runaway, a self-accelerating sequence of exothermic reactions [9]. As a cell heats up, the SEI begins to decompose at around 80–120 °C. The separator then softens and shrinks, allowing internal short circuits. Layered-oxide cathodes decompose and release oxygen, which feeds combustion of the flammable electrolyte. Temperatures can climb to several hundred degrees within seconds. LFP is markedly more tolerant because the strong covalent phosphorus–oxygen bonds of its olivine structure hold oxygen far more tightly. At pack level, the engineering goal is to keep the failure of one cell from spreading to its neighbours, using thermal barriers, controlled vent paths and careful cell spacing. Regulators are raising the bar: China’s GB 38031-2025 standard, applied to new vehicle type approvals from July 2026, requires that a thermal runaway in the pack lead to no fire or explosion [10].
Degradation is slower but unavoidable. The principal mechanisms are loss of lithium inventory as the SEI grows; loss of active material through particle cracking, which is in essence fatigue driven by the cyclic intercalation strain; and lithium plating on the anode during fast charging or at low temperatures [11]. High temperatures and long periods at high state of charge accelerate ageing. Real-world data are reassuring, however. A 2024 telematics study of around 5,000 vehicles found average capacity loss of about 1.8% per year, with faster degradation in hot climates and under heavy use of DC fast charging [12]. At that rate, most packs will outlast the vehicles they power. When capacity falls to around 70–80% of its original value, the pack can still find a second life in stationary storage before its materials are recovered through recycling.
Looking Ahead
The battery pack has replaced the fuel tank, but it is far more than a container: it is an electrochemical reactor, a structural member and a heat source, all held within tight safety margins. None of this works without supervision. In the next article, we examine the battery management system (BMS), the electronic “brain” that monitors every cell, estimates state of charge and health, and keeps the pack within its safe operating limits.
References
[1] U.S. Department of Energy, Alternative Fuels Data Center, “Fuel Properties Comparison.”
[2] J. B. Goodenough and K.-S. Park, “The Li-Ion Rechargeable Battery: A Perspective,” Journal of the American Chemical Society, vol. 135, no. 4, pp. 1167–1176, 2013.
[3] N. Nitta, F. Wu, J. T. Lee, and G. Yushin, “Li-ion Battery Materials: Present and Future,” Materials Today, vol. 18, no. 5, pp. 252–264, 2015.
[4] R. Schmuch, R. Wagner, G. Hörpel, T. Placke, and M. Winter, “Performance and Cost of Materials for Lithium-Based Rechargeable Automotive Batteries,” Nature Energy, vol. 3, pp. 267–278, 2018.
[5] International Energy Agency, Global EV Outlook 2025. Paris: IEA, 2025.
[6] M. N. Obrovac and V. L. Chevrier, “Alloy Negative Electrodes for Li-Ion Batteries,” Chemical Reviews, vol. 114, no. 23, pp. 11444–11502, 2014.
[7] Tesla, Inc., “Battery Day” presentation, 22 September 2020.
[8] BYD Company Ltd., “BYD’s New Blade Battery Set to Redefine EV Safety Standards,” press release, March 2020.
[9] X. Feng, M. Ouyang, X. Liu, L. Lu, Y. Xia, and X. He, “Thermal Runaway Mechanism of Lithium Ion Battery for Electric Vehicles: A Review,” Energy Storage Materials, vol. 10, pp. 246–267, 2018.
[10] Ministry of Industry and Information Technology of the People’s Republic of China, GB 38031-2025, Safety Requirements for Power Batteries Used in Electric Vehicles, 2025.
[11] C. R. Birkl, M. R. Roberts, E. McTurk, P. G. Bruce, and D. A. Howey, “Degradation Diagnostics for Lithium Ion Cells,” Journal of Power Sources, vol. 341, pp. 373–386, 2017.
[12] Geotab, “New Geotab Data Highlights How EV Batteries Can Last 20 Years or More,” press release, September 2024.



0 Comments